• influence of the load ratio on the threshold stress intensity factor range for heavily drawn steel wires

    جزئیات بیشتر مقاله
    • تاریخ ارائه: 1390/01/01
    • تاریخ انتشار در تی پی بین: 1390/01/01
    • تعداد بازدید: 499
    • تعداد پرسش و پاسخ ها: 0
    • شماره تماس دبیرخانه رویداد: -
     the fatigue behavior of heavily drawn steel wires with a diameter of 175 μm and total strain of 3.5 has been studied. a new approach is used to estimate the threshold stress intensity factor range for crack growth (δkth,r) which is based on fatigue crack initiations at internal non-metallic inclusions. at these internal crack initiations a characteristic area is formed around the inclusion (in literature this region is called optical dark area, granularly bright facet or facet). this area corresponds to the short crack growth regime. the transition between short and long crack growth, which can be seen clearly by fractography, is used to estimate δkth,r.

سوال خود را در مورد این مقاله مطرح نمایید :

با انتخاب دکمه ثبت پرسش، موافقت خود را با قوانین انتشار محتوا در وبسایت تی پی بین اعلام می کنم
مقالات جدیدترین رویدادها
مقالات جدیدترین ژورنال ها